Chemical composition % of the ladle analysis of grade Z6CNDT17-12
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | Ti(%) |
Max 0.06 | Max 0.75 | Max 2.00 | Max 0.040 | Max 0.015 | 16.0-18.0 | 10.5-12.5 | 2.00-2.50 | Max 0.020 | 5(C+N)Max 0.70 |
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
852 (≥) | 484 (≥) | 41 | 33 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
125 (≥) | 183 (≥) | 24 | 11 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
289 | 344 | 529 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |
Grade | Standard | Country | Application |
---|---|---|---|
Z6CNDT17-12 | Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels |
||
Z6CNDT17-12F | General purpose forgings. Stainless steels |
||
TUZ6CNDT17-12 | Steel tubes. Seamless plain end tubes for pipes-lines and other uses. Ferritic and austenitic stainless steels. Dimensions. Technical delivery conditions |