Stainless Steels - Special Steels SUS 347, KSUS347, SUS 347, SUS 347, SUS 347, SUS 347, SUS 347, SUS 347, SUS 347, SUS 347, SUS 347, SUS 347 FB, SUS 347 HFB, SUS 347 HTB, SUS 347 HTF, SUS 347 HTP, SUS 347 TB, SUS 347 TF, SUS 347 TKA, SUS 347 TP, SUS 347 TPY, Cold-rolled stainless steel plate, sheet and strip to G 4305 (2012)
SUS 347 Stainless Steels - Special Steels Properties Data
Chemical Composition of steel SUS 347 Stainless Steels - Special Steels: G 4305 (2012) ,Cross Reference
SUS 347 Stainless Steels - Special Steels Applications and Specifications
Cold-rolled stainless steel plate, sheet and strip
- G 4305 (2012) - Cold-rolled stainless steel plate, sheet and strip
Mechanical properties at room temperature for SUS 347 Stainless Steels - Special Steels: G 4305 (2012)
Tensile Strength,Rm(MPa)
Yield Strength,Rp 0.2(MPa)
Impact,Kv/Ku(J)
Elongation,A(%)
Reduction of area,(%)
Hardness
Product shapes we supply:
Cross Reference, Equivalent, Similar of SUS 347 Stainless Steels - Special Steels grade:
KSUS347
SUS 347
SUS 347
SUS 347
SUS 347
SUS 347
SUS 347
SUS 347
SUS 347
SUS 347
SUS 347 FB
SUS 347 HFB
SUS 347 HTB
SUS 347 HTF
SUS 347 HTP
SUS 347 TB
SUS 347 TF
SUS 347 TKA
SUS 347 TP
SUS 347 TPY
SUS 347FB
SUS 347HFB
SUS 347TP
SUS 347TP Y
SUS 347HTP
SUS 347TKA
Conditions & Properties
- +A Soft annealed
- +AC Annealed to achieve spheroidization of the carbides
- +QT Quenched and tempered
- +WW Warm worked
- +N Normalized
- +NT Normalized and tempered
- +AT Solution annealed
- +C Cold drawn / Hard
- +CR Cold rolled
- +PE Peeled
- +T Tempered