Stainless Steels - Special Steels 17-4PH, A 1028 S17400, A 564 S17400, A 693 S17400, A 705 S17400, A 982 S17400, A 988 S17400, F738 Class P1.90 S17400, F836 Class P1.90 S17400, S17400, SA.564 S17400, SA.693 S17400, SA.705 S17400, 17.4PH, 17.4PH, Z6CNU17.04, 17.4PH, 1.4542, X5CrNiCuNb16.4, Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4) to SAE AMS 5342E (2006)

17-4PH Stainless Steels - Special Steels Properties Data

Chemical Composition of steel 17-4PH Stainless Steels - Special Steels: SAE AMS 5342E (2006) ,Cross Reference

17-4PH Stainless Steels - Special Steels Applications and Specifications

SAE AMS 5342E (2006) Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4)
\
Used typically for parts requiring good corrosion resistance and strength up to 315°C.

  • SAE AMS 5342E (2006) - Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4)
  • SAE AMS 5343E (2006) - Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1000) 150 ksi (1034 MPa) Tensile Strength (17-4)
  • SAE AMS 5344F (2007) - Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H900) 180 ksi (1241 MPa) Tensile Strength (17-4)
  • SAE AMS 5604G (2013) - Steel, Corrosion Resistant, Sheet, Strip, and Plate 16.5Cr - 4.0Ni - 4.0Cu - 0.30Cb Solution Heat Treated, Precipitation Hardenable
  • SAE AMS 5622F (2013) - Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable Consumable Electrode Remelted
  • SAE AMS 5643/H1150 (2013) - Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing and Rings 16Cr – 4.0Ni – 0.30Cb (Nb) – 4.0Cu Solution and Precipitation Heat Treated (H1150)
  • SAE AMS 5643S (2013) - Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable
  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Mechanical properties at room temperature for 17-4PH Stainless Steels - Special Steels: SAE AMS 5342E (2006)

Tensile Strength,Rm(MPa)

Yield Strength,Rp 0.2(MPa)

Impact,Kv/Ku(J)

Elongation,A(%)

Reduction of area,(%)

Hardness

Product shapes we supply:

Cross Reference, Equivalent, Similar of 17-4PH Stainless Steels - Special Steels grade:

A 1028 S17400 A 564 S17400 A 693 S17400 A 705 S17400 A 982 S17400 A 988 S17400 F738 Class P1-90 S17400 F836 Class P1-90 S17400 S17400 SA-564 S17400 SA-693 S17400 SA-705 S17400 17-4PH 17-4PH Z6CNU17-04 17-4PH, 1.4542, X5CrNiCuNb16-4

Conditions & Properties

  • +A Soft annealed
  • +AC Annealed to achieve spheroidization of the carbides
  • +QT Quenched and tempered
  • +WW Warm worked
  • +N Normalized
  • +NT Normalized and tempered
  • +AT Solution annealed
  • +C Cold drawn / Hard
  • +CR Cold rolled
  • +PE Peeled
  • +T Tempered