Chemical composition % of the ladle analysis of grade 15X17AΓl4

Max 0.15 Max 0.80 13.5-15.5 Max 0.035 Max 0.02 16.0-18.0 Max 0.60 Max 0.30 Max 0.20 0.25-0.37 Max 0.20
15X17AΓl4
Mechanical properties of grade 15X17AΓl4
Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
994 (≥) 715 (≥) 33 34 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Physical properties of grade 15X17AΓl4
Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
246 (≥) 958 (≥) 31 21 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
199 298 459
15X17AΓl4 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED
Cross Reference Table(Equivalent Grade)
Grade Standard Country Application
15X17AΓl4
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Enquiry