Structural Steel 08F, 08F, U20082, This standard specifies the alloy steel, low alloy steel, alloy steel chemical composition relative to the provisions of the finished steel smelting chemical composition boundary limit allowable deviation, and gives the definition of related terms. to GB/T 699-1999

08F Structural Steel Properties Data

Chemical Composition of steel 08F Structural Steel: GB/T 699-1999 ,Cross Reference

08F Structural Steel Applications and Specifications

Delivery status: hot or hot forging
This standard specifies the alloy steel, low alloy steel, alloy steel chemical composition relative to the provisions of the finished steel smelting chemical composition boundary limit allowable deviation, and gives the definition of related terms.

ReL (MPa) Rm (MPa) Z (%) A5.65 (%) Heat treatment condition Technology Sampl
175(≥) 295(≥) 60(≥) 35(≥) Normalizing 930℃ Heat preservation≥30min AC Normalizing 25(Sampl size)

HBS: 131(≤)


  • GB/T 699-1999 - This standard specifies the alloy steel, low alloy steel, alloy steel chemical composition relative to the provisions of the finished steel smelting chemical composition boundary limit allowable deviation, and gives the definition of related terms.
  • GB 13237-1991 -
  • GB/T 13793-1992 -
  • GB 3206-1982 -
  • GB/T 711-2008 -
  • GB 3275-1991 -
  • GB 699-1988 -
  • GB 710-1991 -
  • GB 711-1988 -

Mechanical properties at room temperature for 08F Structural Steel: GB/T 699-1999

Tensile Strength,Rm(MPa)

Yield Strength,Rp 0.2(MPa)

Impact,Kv/Ku(J)

Elongation,A(%)

Reduction of area,(%)

Hardness

Product shapes we supply:

Cross Reference, Equivalent, Similar of 08F Structural Steel grade:

08F U20082

Conditions & Properties

  • +A Soft annealed
  • +AC Annealed to achieve spheroidization of the carbides
  • +QT Quenched and tempered
  • +WW Warm worked
  • +N Normalized
  • +NT Normalized and tempered
  • +AT Solution annealed
  • +C Cold drawn / Hard
  • +CR Cold rolled
  • +PE Peeled
  • +T Tempered